Research Article

Influence of Deposition Condition on Y2O3 Coatings Produced by Pulsed Electrophoretic Deposition

Figure 5

Cross-sectional SEM images of films deposited at various bias frequencies (10 Hz, 1 kHz, and 100 kHz), with bias voltage of 0.5 V and Y2O3 concentration of 0.5 wt% in a suspension solution.
(a)
(b)
(c)