Research Article
Microstructure and Mechanical Behavior of Hot Pressed Cu-Sn Powder Alloys
Figure 9
SEM image of irregularity and rough morphology of the fracture surface for (a) compression fractured 85% Cu-10% Sn-5% C alloys, (b) higher magnification showing melting droplets morphology, (c) compression fractured 80% Cu-10% Sn-10% Pb alloys, and (d) higher magnification showing melting droplets morphology.