Properties and Internal Curing of Concrete Containing Recycled Autoclaved Aerated Lightweight Concrete as Aggregate

Table 5

Differential percentage of minute compressive strength in layer 1 (L1) between exterior and interior zone.

MixturesAir curing (AC)Water curing (WC)
L1 7 d (MPa)L1 28 d (MPa)L1 7 d (MPa)L1 28 d (MPa)
Ext.Int.Ext.Int.Ext.Int.Ext.Int.

NC0.640.9548.470.841.3054.130.771.0334.481.211.5427.86
LWA200.831.1234.001.121.6951.101.111.4126.981.482.0135.32
LWA400.931.3039.031.001.5554.991.261.5723.821.321.7330.74
LWA600.931.2332.001.131.6242.931.151.3921.641.431.8025.51