Research Article
Investigation of the Scanning Microarc Oxidation Process
Figure 15
Surface morphology of the A356 alloy after 15 min: (a) and (d) are, respectively, SMAO (interelectrode gap 5 mm, zero velocity) and MAO; (b) and (c) are the high magnification of the dotted rectangle area; (e) and (f) are the high magnification of the dotted rectangle area.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |