Research Article
Investigation of the Scanning Microarc Oxidation Process
Figure 5
Photographs showing thickness variation in an SMAO coating deposited on an A356 aluminum substrate using AC1 and 5 mm interelectrode gap after (a) 5 min and (b) 60 min of treatment.
(a) |
(b) |