Research Article

Optimization of Alumina Slurry for Oxide-Oxide Ceramic Composites Manufactured by Injection Molding

Figure 3

Viscosity at 0.1 s−1 shear rate versus acid content for B33 slurries with varied acid content from 0 to 0.34 wt%.