Research Article

Optimization of Alumina Slurry for Oxide-Oxide Ceramic Composites Manufactured by Injection Molding

Figure 9

Viscosity versus shear rate for B33 base slurry (0.17 wt% acid and 3.80 wt% PVA) preparation using HSM. Consecutive pass in HSM using the same mixture from 1 pass to 10 passes. Slurry with 0 passes corresponds to US.