BET surface area and crystal dimensions calculated from Scherrer’s equation.

SamplesBET surface area (m2/g)Crystallite size (nm)
TiO2WO3

TiW5.1520.819.5
TiW-Nb24.9919.518.0
TiW-Nb44.9420.118.5