Research Article
Experimental Study and Application of Inorganic Solidified Foam Filling Material for Coal Mines
Table 2
Physical parameters of ordinary Portland cement.
| Fineness (0.08 mm, residue on square hole sieve) | Apparent density (kg/m3) | Initial setting time (min) | Final setting time (min) | Compressive strength (MPa) | 1 d | 28 d |
| 8% | 3.06 | 139 | 375 | 12.8 | 46.7 |
|
|