Basic properties of binders with different RAP contents.

Type of binderPenetration/0.1 mmSoftening point/°C25°C ductility/cm

Extracted RAP binder31.360.67.7
Virgin binder68.048.3130.7
25% RAP binder60.552.190.6
50% RAP binder48.855.045.5