The Adhesion of CrN Thin Films Deposited on Modified 42CrMo4 Steel
Table 1
The properties of CrN coatings on 42CrMo4 steel.
| Thickness (μm) | 1.8 ± 0.2 | Hardness, H (GPa) | 23.6 ± 0.8 | Young’s modulus, E (GPa) | 285 ± 8 | H/E index | 0.082 ± 0.005 | Stress, σ (GPa) | −1.4 ± 0.2 |
|
|