Effect of Reduction in Thickness and Rolling Conditions on Mechanical Properties and Microstructure of Rolled Mg-8Al-1Zn-1Ca Alloy
Figure 7
(a) Inverse pole figure maps of the 3 mm thick rolled sample and (b) the grain size distribution diagram. The grain size and area fraction are shown in the IPF maps.