Adhesive Through-Reinforcement Improves the Fracture Toughness of a Laminated Birch Wood Composite
Figure 9
Load-displacement curves during double cantilever beam (DCB) mode I fracture toughness tests of specimens with 6 different levels of through-reinforcement (including the control): (a) reinforcement levels less than 24 (<1.43/cm2); (b) reinforcement levels greater than 39 (>2.33/cm2).
(a) |
(b) |