Research Article
Novel Evaporation Process for Deposition of Kesterite Thin Films Synthesized by Solvothermal Method
Figure 1
SEM images of morphology and sizes of prepared particles, (a) and (e) correspond to samples with 0.324 g of PVP; (b), (c), and (d) correspond to samples with 0.640 g of PVP, and (f), (g), and (h) correspond to samples with 0.964 g of PVP.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |
(h) |