Research Article
Analysis of Startup Process and Its Optimization for a Two-Stand Reversible Cold Rolling Mill
Table 1
Typical rolling schedule for simulation calculation.
| Stand | Entry thickness /mm | Exit thickness /mm | Forward tension /MPa | Back tension /MPa | Rolling speed /m⋅min−1 |
| Entry stand | 3.000 | 2.120 | 126 | 29 | — | Exit stand | 2.120 | 1.417 | 84 | 126 | 574 |
|
|