Estimation of Oxidation Kinetics and Oxide Scale Void Position of Ferritic-Martensitic Steels in Supercritical Water

Figure 7

Comparison of the thickness of oxide scale of final superheater tubes during the oxidation of T91 for different exposure time among field measurement data, simulation results, and calculation results according to Sabau and Wright’s method [26].