Research Article

Oxidation Resistance and Modification Reaction Mechanism of Al Coating Sprayed on Pure Ti Substrate

Figure 6

(a) Cross-sectional BSD image of Al coating after testing for 5 hours at 1073 K, (b) the expanded view of region I in Figure 6(a), (c) EDS results of points A and B in Figure 6(b), and (d) EDS results of points C and D marked in Figure 6(b).