Properties and process parameters of the blank tube.
| Tube material | Elastic modulus (MPa) | Poisson’s ratio | Yield stress () | Outside diameter of tube (mm) | Tube-wall thickness (mm) | R (mm) | Δt (mm) | f (mm/r) |
| Magnesium alloy (AZ31B) | 44800 | 0.31 | 180 | 18 | 1.5 | 2.5 | 0.1 | 0.1 | 3 | 0.2 | 0.15 | 3.5 | 0.3 | 0.2 | 4 | 0.4 | 0.25 | 4.5 | 0.5 | 0.3 |
|
|