Research Article
Influence of Processing Parameters on Laser Direct Joining of CFRTP and Stainless Steel
Figure 16
The morphology of debonding surface of the stainless steel/CFRTP joints with different PPS addition thickness after tensile: (a) 0, (b) 150 μm, (c) 300 μm, and (d) 450 μm.
(a) |
(b) |
(c) |
(d) |