Research Article
Porogenic Behavior of Water in High-Alumina Castable Structures
Figure 3
Effects of water content (W vol.%) on samples’ total porosity (TP, %) and flexural elastic modulus (E GPa) after conventional static curing and drying at 120°C for 24 h.