Study of Thermomechanical Properties of an Al-Zn-Based Composite Reinforced with Dodecaboride Particles

Figure 3

Typical Al-Zn matrix composite deformation curves at 125°C, 125°C, and 125°C as a function of time for (a) 5 wt.% Zn and (b) 10 wt.% Zn (triangles = 0 vol.% , circles = 16.5 vol.% , and squares = 22.5 vol.% ).