Research Article

Service Life Prediction of Shaft Sidewall Exposed to Sulfate Environment

Table 3

The major performance of the PO 42.5R cement.

80 μm sieve residueWater requirementInitial setting timeFinal setting timeFlexural strengthCompressive strength
3 d28 d3 d28 d

0.6%0.268180 min320 min3.57.525.248.4