Research Article
Influence of Deformation Conditions on the Critical Damage Factor of AZ31 Magnesium Alloy
Figure 7
Variation in the damage sensitive rate on the outer edge of the upsetting drum at different temperatures and strain rates. Greater details of the graphs from (a)–(c) above 40 increment steps are shown in insets. (a); (b); (c).
(a) |
(b) |
(c) |