Research Article
Behaviors of Oxide Film during Semisolid Brazing of SiCp/6063Al Composite Materials
Figure 5
The microstructure of the filler metal heated to different temperatures without compression: (a) 382°C; (b) 386°C; (c) 392°C; (d) 410°C.
(a) |
(b) |
(c) |
(d) |