Research Article
Mechanical Performance of Zr-Containing 354-Type Al-Si-Cu-Mg Cast Alloy: Role of Additions and Heat Treatment
Figure 2
Optical micrographs at 500X showing the morphology of the eutectic silicon in the alloys studied: (left) as-cast conditions and (right) solution heat-treated conditions: (a) as-cast alloy M1S, (b) SHT alloy M1S, (c) as-cast alloy M2S, (d) SHT alloy M2S, (e) as-cast alloy M3S, (f) SHT alloy M3S, (g) as-cast alloy M4S, (h) SHT alloy M4S, (i) as-cast alloy M5S, and (j) SHT alloy M5S.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |
(h) |
(i) |
(j) |