Advances in Materials Science and Engineering / 2018 / Article / Fig 8

Research Article

Fracture Toughness Improvement of Poly(lactic acid) Reinforced with Poly(ε-caprolactone) and Surface-Modified Silicon Carbide

Figure 8

SEM micrographs of PLA/PCL/SiC composites after KIC tests: (a) PLA/PCL (2.5 wt.% PCL); (b) 0.25 wt.% SiC; (c) 0.5 wt.% SiC; (d) 0.75 wt.% SiC; (e) 1.0 wt.% SiC (magnification of 5000).
(a)
(b)
(c)
(d)
(e)

We are committed to sharing findings related to COVID-19 as quickly and safely as possible. Any author submitting a COVID-19 paper should notify us at help@hindawi.com to ensure their research is fast-tracked and made available on a preprint server as soon as possible. We will be providing unlimited waivers of publication charges for accepted articles related to COVID-19. Sign up here as a reviewer to help fast-track new submissions.