Effects of Alloying Elements (Cr, Mn) on Corrosion Properties of the High-Strength Steel in 3.5% NaCl Solution

Figure 5

XRD patterns of the adherent rust (AR) formed on (a) REF, (b) 18Mn, and (c) 18Mn5Cr for 56 days in 3.5% NaCl solution at 60°C, where S represents magnetite (or maghemite).