Research Article
Influence of Thermal Parameters, Microstructure, and Morphology of Si on Machinability of an Al–7.0 wt.% Si Alloy Directionally Solidified
Figure 7
(a) Image of different tools used on necking tests: (1) before and (2) after removing false edge, showing flank wear. (b) Maximum flank wear as a function of secondary dendrite arm spacings.