Research Article
Experimental Investigation on Flexural Behavior of Granite Stone Slabs with Near Surface Mounted CFRP Bars and Screw-Thread Steels
Table 2
Tensile splitting strength results for granite.
| Number of specimen | Specimen dimensions (D × H/mm) | Failure loading (kN) | Tensile splitting strength (MPa) | Average value (MPa) |
| 1 | 50 mm × 50 mm | 38.4 | 9.98 | 8.94 ± 0.79 | 2 | 37.2 | 9.67 | 3 | 36.7 | 9.54 | 4 | 31.9 | 8.12 | 5 | 33.0 | 8.57 | 6 | 29.8 | 7.74 |
|
|