Research Article
Synthesis of Ti2SnC under Optimized Experimental Parameters of Pressureless Spark Plasma Sintering Assisted by Al Addition
Figure 5
XRD pattern and SEM of the sample with molar ratio 2 : 1 : 0.2 : 1 at 1400°C sintering temperature on pressure of (a) 0 and (b)100 MPa.