The average thickness of each specimen before and after the test.
| Specimens | Tests | Measuring points (cm) | Average thickness (cm) | 1 | 2 | 3 | 4 | 5 |
| FM-0 | Before | 0.5981 | 0.5962 | 0.6039 | 0.6045 | 0.6038 | 0.6013 | After | 0.5517 | 0.5504 | 0.5578 | 0.5585 | 0.5582 | 0.5553 |
| FM-1 | Before | 0.6017 | 0.6017 | 0.5992 | 0.6004 | 0.6026 | 0.6011 | After | 0.5482 | 0.5470 | 0.5448 | 0.5456 | 0.5484 | 0.5468 |
| FM-3 | Before | 0.5989 | 0.5988 | 0.5997 | 0.5992 | 0.6012 | 0.5995 | After | 0.5487 | 0.5472 | 0.5461 | 0.5467 | 0.5486 | 0.5474 |
| FM-5 | Before | 0.6013 | 0.6012 | 0.6010 | 0.6008 | 0.6013 | 0.6011 | After | 0.5497 | 0.5492 | 0.5486 | 0.5492 | 0.5506 | 0.5495 |
| FM-7 | Before | 0.5997 | 0.5998 | 0.5995 | 0.5999 | 0.6008 | 0.5999 | After | 0.5528 | 0.5528 | 0.5519 | 0.5524 | 0.5530 | 0.5526 |
| FM-9 | Before | 0.6001 | 0.5996 | 0.6003 | 0.5997 | 0.6004 | 0.6000 | After | 0.5527 | 0.5522 | 0.5527 | 0.5520 | 0.5526 | 0.5524 |
|
|