Research Article
Effect of Heat Treatment and Titanium Addition on the Microstructure and Mechanical Properties of Cast Fe31Mn28 Ni15Al24.5Tix High-Entropy Alloys
Figure 9
Micrographs of the 20 h heat-treated samples: (a) C1, (b) C2, and (c) C3 at 30 mm and (d) C1 at 5 mm.
(a) |
(b) |
(c) |
(d) |