Research Article
Three-Point Bending Fatigue Test of TiAl6V4 Titanium Alloy at Room Temperature
Figure 4
The microstructure of experimental material—TiAl6V4 alloy: (a) the grain length measurement, (b) the width of grains measurements, and (c, d) α—lamellae measurements, 10% HF acid etching.
(a) |
(b) |
(c) |
(d) |