Research Article
Three-Point Bending Fatigue Test of TiAl6V4 Titanium Alloy at Room Temperature
Figure 9
Details of transcrystalline cleavage failure of TiAl6V4 grains: (a) transcrystalline cleavage facet with river morphology; (b) transcrystalline cleavage failure of grains with a higher degree of cleavage, SEM.
(a) |
(b) |