Research Article

Titanium Alloy Repair with Wire-Feed Electron Beam Additive Manufacturing Technology

Figure 18

Fatigue life curves for the SRed Ti6Al4V wall deposit and SRed wrought Ti6Al4V tested at room temperature, R = 0.1 and 6 Hz. The superimposed fatigue performance of unnotched Ti6Al4V (tested at R = 0.1) for wrought, cast plus HIP, and cast products were reproduced from [50].
(a)
(b)