Research Article
Study on Surface Hardness and Microstructure of Pure Copper Chip Strips Prepared by LSEM
Table 1
Experiment and simulation parameters.
| Cutting condition | Chip thickness compression ratio λ | Rake angle α (°) | Uncut chip thickness t0 (mm) |
| C1 | 1.5 | 15 | 0.6 | C2 | 1.5 | 20 | 0.6 | C3 | 1.5 | 30 | 0.6 | C4 | 1.5 | 20 | 0.6 | C5 | 2 | 20 | 0.6 | C6 | 2.5 | 20 | 0.6 | C7 | 1.5 | 20 | 0.4 | C8 | 1.5 | 20 | 0.6 | C9 | 1.5 | 20 | 0.8 |
|
|