Research Article

Study on Surface Hardness and Microstructure of Pure Copper Chip Strips Prepared by LSEM

Table 7

Experimental results for surface hardness.

No.DEEmpty columnFSurface hardness (HV)

11111134.5
21222127.0
31333122.2
42123114.2
52231118.2
62312112.2
73132114.6
83213117.6
93321117.3
K1383.7363.3364.3370.0T = 1077.8
K2344.6362.8358.5353.8 = 129072.5
K3349.5351.7355.0354.0
K1127.9121.1121.4123.3
K2114.9120.9119.5117.9
K3116.5117.2118.3118.1
R13.03.93.15.4
SS302.528.714.757.6