Research Article

Impact of High-Velocity Oxy-Fuel ZrO2 Coating on Corrosion Resistance and Fatigue Life of AISI 316L Austenitic Stainless Steel

Table 11

Fatigue life (cycles) of ZrO2-coated 316L austenitic stainless steel corroded specimen.

RunFactor x1Factor x2Test conditionsFatigue life (cycles)
Trial 1Trial 2

111Stress 250 (MPa)
Strain amplitude 0.4%
Strain rate 3 × 10−3 s−1
98959900
21299309940
32199359945
42299489950