Research Article
Impact of High-Velocity Oxy-Fuel ZrO2 Coating on Corrosion Resistance and Fatigue Life of AISI 316L Austenitic Stainless Steel
Table 6
Fatigue life (cycles) of ZrO2-coated AISI 316L austenitic stainless steel specimen.
| Run | Factor x1 | Factor x2 | Test conditions | Fatigue life (cycles) | Trail 1 | Trial 2 |
| 1 | 1 | 1 | Stress 250 MPa Strain amplitude 0.4% Strain rate 3 × 10−3 s−1 | 10692 | 10685 | 2 | 1 | 2 | 10740 | 10745 | 3 | 2 | 1 | 10710 | 10712 | 4 | 2 | 2 | 11000 | 11020 |
|
|