Study on the Process Optimization and Wear Resistance of Electron Beam Cladding WC-CoCr Coating on Inconel 617 Surface
Figure 8
The curve of the friction coefficient varies with time of Inconel 617 alloy matrix and cladding at 200°C, 600°C, and 1000°C.