Features of Plasma Electrolytic Formation of Manganese- and Cobalt-Containing Composites on Aluminum Alloys
Figure 8
The surface morphology of oxide coatings formed on the alloy A2024 in a solution of 1.0 mol/dm3 K4P2O7, during PEO at time intervals. (a) 5 minutes; (b) 7 minutes; (c) 10 minutes; (d) 30 minutes. Magnification ×1000.