Research Article
Features of Plasma Electrolytic Formation of Manganese- and Cobalt-Containing Composites on Aluminum Alloys
Figure 9
The content of the main alloying components in the surface layer of the alloy A2024: in the initial state (a) and after PEO in solution 1.0 mol/dm3 K4P2O7 within 30 minutes (b).