Research Article
Fretting Wear Behavior and Damage Mechanisms of Inconel X-750 Alloy in Dry Contacts
Figure 3
SEM images of worn scars on Inconel X-750 alloy after (a) 10, (b) 30, and (c) 90 minutes of fretting tests. Double arrow indicates fretting direction.
(a) |
(b) |
(c) |