Research Article
Fretting Wear Behavior and Damage Mechanisms of Inconel X-750 Alloy in Dry Contacts
Figure 5
Surface topographies of worn scars for (a) 40 µm (left) and 100 µm (right) after 90 minutes of fretting test; (b) corresponding preprocessed input area; and (c) selected worn area to calculate the wear volume.
(a) |
(b) |
(c) |