Research Article

Evaluation of Compression Performance of APM Aluminum Foam-Polymer Filled Pipes Prepared via Different Epoxy Resin Bonding Processes

Table 4

Specific energy absorption of each specimen.

Specimen numberThin-walled pipes, J (g/cm3)Epoxy-bonding APM foam filled pipes, J (g/cm3)Epoxy foam-bonding APM composite pipes, J (g/cm3)

1#85.092501.252666.26
2#78.162527.012557.58
3#66.332376.292648.21
4#67.062443.642571.25
5#69.712445.192554.29
SAEaverage73.272458.432600.22

Note. Specific energy absorption = AE/density.