Research Article

Effect of Sterilization on the Properties of a Bioactive Hybrid Coating Containing Hydroxyapatite

Figure 8

SEM/FEG micrographs of the nonsterilized and the sterilized (by three different processes) coatings immersed for 24 and 672 hours in SBF at 37 ± 3°C.