Research Article
Crystal Structure, Lattice Strain, Morphology, and Electrical Properties of SnO2 Nanoparticles Induced by Low Calcination Temperature
Figure 4
The SEM images of investigated SnO2 powder calcined under (a) 300°C, (b) 350°C, (c) 400°C, and (d) 450°C.
(a) |
(b) |
(c) |
(d) |