Research Article
Effects of Anodization-Assisted Electrodeposition Conditions on the Fabrication of CuO-Cu2O Coatings on Nanoporous Stainless Steel
Table 1
Electrodeposition experiment parameters of CuO-Cu2O/NPSS.
| Number | Temperature | Electrolyte concentration |
| A | 20 | 0.02 M Cu(CH3COO)2 · H2O + 0.1 M CH3COONa | B | 20 | 0.1M Cu(CH3COO)2 · H2O + 0.1 M CH3COONa | C | 60 | 0.02 M Cu(CH3COO)2 · H2O + 0.1 M CH3COONa | D | 60 | 0.1M Cu(CH3COO)2 · H2O + 0.1 M CH3COONa |
|
|