Technical index of emulsified asphalt.

PropertiesUnitTest resultSpecification [13]

Particle chargeCationicCationic
Residue on the 1.18 mm sieve%0.076≤0.1
Wrap ratio with coarse aggregate0.86≥2/3
Saybolt viscosity (25°C)S616∼100
Penetration (5 s, 100 g, 25°C)0.1 mm7945∼150
Ductility (15°C)Cm74≥40
Storage stability (1 days, 25°C)%0.7≤1
Storage stability (5 days, 25°C)%4.1≤5