Porosity results of MK-cemented silty clay.

Curing time (d)MK content (%)Porosity (%)

1025.84
222.92
426.21
6

3024.77
222.52
425.80
6

7024.23
221.88
425.44
6

14023.85
221.67
424.78
627.89

28023.25
221.22
424.31
627.12